The thermal behavior of mono (2-ethylhexyl) phthalate (monoester) was investigated in a batch system over the temperature range from 80 to 250°. After a 12 hr reaction period, around 7% of the monoester was decomposed at 80°. The decomposition reached 50% at 150°and 90% at 250°. The reaction products were bis (2-ethylhexyl) phthalate (BEHP ; 53% at 200°), 2-ethylhexanol and phthalic anhydride. The monoester reacted poorly with water, under-going hydrolysis only with difficulty. In addition, cis-elimination did not occur. The mechanism of the decomposition is discussed. 