Title
Wood properties of Eucalyptus globulus at three sites in Western Australia: effects of fertiliser and plantation stocking
Author(s)
Downes, G; Harwood, C; Washusen, R; Ebdon, N; Evans, Rob; White, Don; Dumbrell, Ian; ,
Year
2014
Is Peer Reviewed?
Yes
Journal
Australian Forestry
ISSN:
0004-9158
Publisher
TAYLOR & FRANCIS AUSTRALIA
Location
MELBOURNE
Page Numbers
179-188
DOI
10.1080/00049158.2014.970742
Web of Science Id
WOS:000346472500007
Abstract
Wood properties of 10-year-old trees in Eucalyptus globulus plantations at three sites in Western Australia were examined. Silvicultural treatments applied at age two years were stocking (unthinned, 1250stems ha(-1); thinned to 600stems ha(-1) or 300stems ha(-1)) and nitrogen fertiliser application (0 or 250kg ha(-1) elemental nitrogen) in factorial combination. The three sites differed markedly in their annual rainfall (620-1100mm), open-pan evaporation and soil water-holding capacity. Wood cores were collected at breast height from a total of 263 trees (~15 trees for each site-by-treatment combination), and radial samples prepared for analysis by SilviScan to produce radial profiles of air-dry density and microfibril angle (MFA) and modulus of elasticity (MOE), and by radial near infrared (NIR) surface scanning to produce radial profiles of NIR-predicted Kraft pulp yield (KPY) and cellulose content (CC). Sampling interval was 0.025mm for density and 5mm for the other properties. For wood property mean values (i.e. wood property averages of each pith-to-cambium sample), sites differed significantly only in air-dry density. The Boyup Brook site, which had low annual rainfall, the lowest climate wetness index and soil water-storage capacity and the slowest diameter growth, had the highest mean wood density (648kgm(-3)), while Scott River, with the highest rainfall, had mean density that was 10% lower. The Wellstead site (low rainfall but highest soil water-storage capacity) was intermediate for density. The only other significant differences for mean wood properties were caused by fertiliser addition, which reduced NIR-predicted KPY from 54.6% (without fertiliser) to 54.1% and predicted CC from 43.7% to 43.1%. Clear radial trends were evident for all wood properties. Density, MOE, KPY and CC all increased from pith to the cambium, while MFA declined. From the innermost (pith) 10% to the outermost (cambial) 10% of the radius, density increased on average by 21%, MOE by 103%, KPY by 9% and cellulose by 11%, while MFA declined by 47%. NIR calibrations developed using the SilviScan and NIR spectral data explained 71% of variance in MOE for an independent set of radial wood samples of E. globulus from Victoria, but less than 50% of variance for density and MFA. Implications for paper pulp and veneer manufacture are briefly considered.