CHROMIUM-MANGANESE ALLOY PLATING 
Sriveeraraghavan, S; Parthasaradhy, NV; Krishnan, RM; Natarajan, SR; Udupa, HVK 
1981 
Metal Finishing
ISSN: 0026-0576 
79 
11 
57-62 
Bath compositions capable of yielding Cr-Mn alloy deposits with manganese content from 4. 8 to 9. 6% at 20 degree C and at current densities of 500-1500 A/m**2. The particular, exports deposits of Cr-Mn alloys produced under optimum conditions were smooth, uniform in appearance and plate with about the same current efficiency as unalloyed Cr.